Xi'an Taijin Industrial Electrochemical Technology Co., LTD.
|
Gold Index: 122077
Price: | 1.0 USD |
Payment Terms: | T/T,L/C,WU,Paypal,Money Gram |
Place of Origin: | Shaanxi, China (Mainland) |
Add to My Favorites | |
HiSupplier Escrow |
Titanium MMO Ribbon Anode for Protection of Storage Tanks Base
Xi'an Taijin Supply mmo titanium anodes in the form of ribbon for the protection of external bases of above-ground storage tanks, and consists of a proprietary mix of Iridium and tantalum oxide titanium base metal confirm to ASTM B265 standard.
MMO Ribbon Anodes are suitable for joining to titanium conductor bar by spot welding to form a grid pattern under the tank which provide the even distribution of current. The anodes are suitable for direct burial in fine sand without carbonaceous backfill.
1. Substrate&Coating
Titanium ASTM B265 Grade1
1)Composition
C | max 0.08% |
N | max 0.03% |
H | max 0.015% |
Fe | max 0.20% |
O | max 0.18% |
Residual | max each 0.1% |
Residual | max total 0.4% |
Ti | balance |
2)Coating:MixedMetal Oxide-IrO2+Ta2O5
2. Dimensions&Parameters
Width(mm) Thickness Length CurrentOutput ExpectedLife(Y)
6.35 0.635(mm) 152/100(m) 17(mA/m) 50
6.35 0.635(mm) 152/100(m) 42(mA/m) 50
3.Application
1) Undertank protection
2) Internal tank protection
3) Aboveground storagetanks.
4.The Third Party Test Certificates.
Test Cetificates from Det Norske Veritas (U.S.A.), Inc. Under NACE TM0108-2008
Production Assessment from Bureau Veritas
5. Quality Assurance and Control
Strict quality procedures are followed throughout the whole process from raw materials to finished products to ensure coating adhesion and loading.
1) Chemical Composition- ASTM B265 Gr1
Element | Content % |
Nitrogen | 0.03 Max |
Carbon | 0.08 Max |
Hydrogen | 0.015 Max |
Iron | 0.2 Max |
Oxygen | 0.18 Max |
Residual(each) | 0.1 Max |
Residual(total) | 0.4 Max |
Titanium | Balance |
2) Visual Coating Uniformity, Color and Scratch
3) Coating adhesion
Three Steps
First, feeling the surface of tubular anodes in a pair of white gloves to observe
whether black mark is left on the gloves
Second, paste with transparent tape to observe whether black mark is left on the
Tape
Third, bend the ribbon to observe whether the coating fades
4) Accelerate Life Test
NACE standard TM0294-2007, 15000A/m2, 1mol/l Na2SO4
6. Workshop
Automatic and Continuous Ribbon Furnace
Accerlerate Life Test
Coating Thickness Test
7.Products:
Raw Materials
Xi'an Taijin Industrial Electrochemical Technology Co., LTD. [China (Mainland)]
Business Type:Manufacturer
City: Xi'an
Province/State: Shaanxi
Country/Region: China (Mainland)