MMO Mesh Ribbon Anode
Mixed Metal Oxide (MMO) Mesh is a durable anode designed for ImpressedCurrent Cathodic Protection systems of steel structures and steel reinforcement concrete. The MMO coating, with industrially proven lifetime characteristics,ensures an even current distribution.
1. Substrate & Coating
Titanium ASTM B265 Grade 1
1)Composition
C | max 0.08% |
N | max 0.03% |
H | max 0.015% |
Fe | max 0.20% |
O | max 0.18% |
Residual | max each 0.1% |
Residual | max total 0.4% |
Ti | balance |
2)Coating: Mixed Metal Oxide-IrO2+Ta2O5
2.Parameters:
1)Other specification can be availableas client's requirement.
width (mm) | length (m) | thickness (mm) | Current Rating | surface area (m2) | mesh dimension (mm) |
10 | 76 | 1.3 | 2.8ma/m | 1.85 | 2.5x4.6 x0.6 |
13 | 76 | 1.3 | 3.5ma/m | 2.4 | 2.5x4.6 x0.6 |
19 | 76 | 1.3 | 5.28ma/m | 3.6 | 2.5x4.6 x0.6 |
1220 | 76 | 1.98 | 37.8ma/m2 | 92.9 | 25x50 x0.89 |
1220 | 76 | 1.98 | 24.4ma/m2 | 92.9 | 34x76x0.89 |
2) Anode Performance:
Current Rating at 100 mA/m2(10mA/ft2) | 2.8mA/m(0.085mA/ft) |
Expected life(NACE Standard TM02944-94) | 100years |
Catalyst | Mixed Metal Oxide(MMO) |
Maximum anode concrete interface current density: | |
FHWA limit | 110mA/m2(10mA/ft2) |
Short-term limit | 220mA/m2(20mA/ft2) |
3.Application
Reinforced concrete, Bridge,Pier Floodcontrolembankment;
4. The Third Party Certificate
Test Cetificates from Det Norske Veritas (U.S.A.), Inc. Under NACE TM0108-2008
Production Assessment from Bureau Veritas
5. Quality Assurance
7. Quality Assurance of MMO Mesh Ribbon
Strict quality procedures are followed throughout the whole process from raw materials to finished products to ensure coating adhesion and loading.
1) Chemical Composition- ASTM B265 Gr1
Element | Content % |
Nitrogen | 0.03 Max |
Carbon | 0.08 Max |
Hydrogen | 0.015 Max |
Iron | 0.2 Max |
Oxygen | 0.18 Max |
Residual(each) | 0.1 Max |
Residual(total) | 0.4 Max |
Balance |
2) Visual Coating Uniformity, Color and Scratch
3) Coating adhesion
Three Steps
First, feeling the surface of tubular anodes in a pair of white gloves to observe
whether black mark is left on the gloves
Second, paste with transparent tape to observe whether black mark is left on the
Tape
Third, bend the ribbon to observe whether the coating fades
4) Accelerate Life Test
NACE standard TM0108-2008, 15000A/m2, 1mol/l Na2SO4
8. Products
Raw Materials
Half-finishedProducts
Finished Items
Packages
Xi'an Taijin Industrial Electrochemical Technology Co., LTD. [China (Mainland)]
Business Type:Manufacturer
City: Xi'an
Province/State: Shaanxi
Country/Region: China (Mainland)